2016 №08 |
DOI of Issue https://doi.org/10.15407/as2016.09 |
2016 №10 |

CONTENTS
SCIENTIFIC AND TECHNICAL
- Gajvoronsky A.A., Poznyakov V.D., Markashova L.I., Berdnikova E.N. and Yashchuk V.Ya. Brittle fracture resistance of HAZ metal in arc-welded joints of high-strength steels with carbon content of 0.55–0.65 % ... 3 https://doi.org/10.15407/as2016.09.01
- Prilutsky V.P., Shvab S.L., Petrichenko I.K., Akhonin S.V., Rukhansky S.B. and Radkevich I.A. Argon arc welding of titanium VT22 alloy using filler flux-cored wire ... 10 https://doi.org/10.15407/as2016.09.02
- Tsybulkin G.A. Effect of parameters of welding circuit on formation of welding current pulses ... 15 https://doi.org/10.15407/as2016.09.03
- Korzhik V.N., Lyutik N.P., Chajka A.A., Tkachuk V.I., Gos I.D. and Nikityuk Yu.A. Supersonic electric arc spraying of critical parts of rolling stock of railway transport ... 20 https://doi.org/10.15407/as2016.09.04
- Stefaniv B.V. Investigation of wear resistance of protective coatings under conditions of hydroabrasive wear ... 29 https://doi.org/10.15407/as2016.09.05
- Markashova L.I., Onatskaya N.A. and Demidenko L.Yu. Effect of current pulses on activation of welded surfaces of plates from dissimilar metals (steel 20 + copper M1) ... 33 https://doi.org/10.15407/as2016.09.06
INDUSTRIAL
- Golyakevich A.A., Orlov L.N., Malinov L.S. and Titarenko V.I. Experience in application of electric arc surfacing with flux-cored wire at the enterprises of Ukraine ... 37 https://doi.org/10.15407/as2016.09.07
- Gnatenko M.F. Technological properties of covering masses of electrode coatings ... 42 https://doi.org/10.15407/as2016.09.08
- Knysh V.V., Solovej S.A., Nyrkova L.I., Shitova L.G. and Kadyshev A.A. Influence of corrosion damage on cyclic fatigue life of tee welded joints treated by high-frequency mechanical peening ... 46 https://doi.org/10.15407/as2016.09.09
- Skulsky V.Yu., Tsaryuk A.K., Gavrik A.R., Nimko M.A. and Strizhius G.N. Selection of modes of high-temperature tempering of heat-resistant steel welded joints made by electrodes Thermanit MTS616 ... 52 https://doi.org/10.15407/as2016.09.10
- Dmitrik V.V., Glushko A.V. and Grigorenko S.G. Features of pore formation in welded joints of steam lines in long-term operation ... 56 https://doi.org/10.15407/as2016.09.11
- Lukianenko A.O. and Demetskaya A.V. Modern approaches to performance of toxicological and hygienic studies of welding fumes (Review) ... 61 https://doi.org/10.15407/as2016.09.12
NEWS
- LLC «Fronius Ukraine» — 25 years in Ukraine ... 67
- The 12th International Conference on electron beam technologies «EBT-2016» ... 69
- Our congratulations (K. A. Yushchenko was awarded with the Order of Prince of Yaroslav the Wise IV degree) ... 70