Decrease in structural heterogeneity of incomplete refining region of the HAZ of elded joints in pearlitic steels

V.V. Dmitrik, A.N. Pashchenko

Ukrainian Engineering Academy, Kharkiv, Ukraine

Abstract
Intensity of initiation and development of damage at creep of welded joints in heat-resistant steels is shown to depend upon the kind of initial metal structure in incomplete refining region. Control of temperature conditions of the latter can provide improvement of operational reliability of welded joints.
Keywords: automatic welding, pearlitic steels, welded joints, microdamage, initial structure, structural heterogeneity, steam pipelines

References

1. Zemzin, V.N. (1972) Heat resistance of welded joints. Leningrad: Mashinostroenie.
2. Khromchenko, F.A. (1982) Reliability of welded joints in tubes, boilers and steam pipelines. Moscow: Energoizdat.
3. Shron, R.Z., Nebesova, I.F. (1971) Structure, phase composition and long-time strength of chrome-molybdenum weld metal. Avtomatich. Svarka, 11, 9–11.
4. Khromchenko, F.A. (2002) Service life of steam pipeline welded joints. Moscow: Mashinostroenie.
5. Dmitrik, V.V., llienko, N.A., Kirichenko, E.P. (1991) Improvement of metal mechanical properties of incomplete re¬fining zone. Svarochn. Proizvodstvo, 1, 11–12.
6. Berezina, T.G., Borodina, E.R., Ashikhmina, L.A. et al. (1974) Fine structure of heat-affected zone in welding of 15KMM1F steel. Avtomatich. Svarka, 12, 19–22.
7. Miller, K. (1986) Creep and fracture. Moscow: Metallurgiya.
8. Dmitrik, V.V. (2000) Simulation of structure of heat-resistant pearlite steel welded joint. Avtomatich. Svarka, 4, 27–30.
9. Kumanin, V.I., Kovalyova, L.A., Alekseev, S.V. (1988) Metal service life in creep conditions. Moscow: Metallurgiva.
10. Kasatkin, B.S., Kareta, N.L., Vakhnin, Yu.N. et al. (1958) «White» strip in 15KMM1F steel welded joints. Avtomatich. Svarka, 12, 12–16.
11. Diachenko, S.S., German, S.L, Pavlyak, Ya.S. (1960) Investigation of softening zone produced in welding of steels. Metallovedenie i Term. Obrab. Metallov, 7, 24–26.
12. Tsaryuk, A.K. (1999) Peculiarities of phosphorus influence on size of non-metallic inclusions and properties of heat-resistant steel welded joints. Avtomatich. Svarka, 4, 26–30.
13. Gotalsky, Yu.N. (1981) Welding of dissimilar steels. Kyiv: Tekhnika.
14. Rozenberg, V.M. (1967) Creep of metal. Moscow: Metallurgiva.
15. Khromchenko, F.A., Kalugin, R.N., Lappa, V.A. et al. (1999) Peculiarities of structural changes in welded joints of steel 15KMM1F at creep. Svarochn. Proizvodstvo, 10, 12–15.
16. Khromchenko, F.A., Lappa, V.A., Fedina, I.V. et al. (1998) Influence of technological and metallurgical heredity on damage of 15KMM1F steel welded joint zones under creep conditions. Ibid., 4, 18–21.
17. Fomina, O.P., Gavranek, V.V., Diachenko, S.S. et al. (1965) On nature of a white strip in welded joints. Metallovedenie i Term. Obrab. Metallov, 1, 46–47.
18. Fomina, O.P., Gavranek, V.V., Diachenko, S.S. et al. (1965) Simulation of white strip in welded joints. Svarochn. Proizvodstvo, 3, 13–14.
19. Fomina, O.P., Gavranek, V.V., Diachenko, S.S. et al. (1965) Hardness of white strip in welded joints. Ibid., 11, 5–8.
20. Dmitrik, V.V. (1999) A method of determining the temperature conditions in the molten pool. Welding Int., 2, 159–161.
21. Dmitrik, V.V. (1999) Stabilisation of conditions of automatic welding of pearlite steels. Svarochn. Proizvodstvo, 5, 11–14.
22. (1972) Metallography of iron. Part 2. Structure of steels with microphotograph atlas. Ed. by F.N. Tavadze. Moscow: Metallurgiva.
23. Krutasova, E.L (1981) Reliability of metal of power equipment. Moscow: Energoizdat.
24. Elpanova, N.V., Berezina, T.G. (1989) Influence of structure on kinetics of fracture of 12KMM1F steel at creep. Metallovedenie i Term. Obrab. Metallov, 7, 36–39.