Print
2005 №07 (04) 2005 №07 (06)


The Paton Welding Journal, 2005, #7, 24-27 pages

On concept of pore initiation in welded joints under low-temperature creep

V.V. Dmitrik1, A.I. Konyk2

1Ukrainian Engineering-Pedagogical Academy, Kharkov, Ukraine
2Open Joint Stock Company «Zavod Elektromekhanicheskikh Izdelij», Kharkov, Ukraine

Abstract
It has been found that initiation of pores in welded joints of heat-resistant pearlitic steels and their initial evolution under conditions of low-temperature service creep is mostly of a diffusion character, while their further development is of a dislocation character.
Keywords: thermostable steels, welded joints, pore initiation, carbides, creep, failure, service life

References

1. Paton, B.E. (2003) Current trends of research and development in the field of welding and strength of structures. The Paton Welding J., 10/11, 5–11.
2. Makhnenko, V.I. (2003) Improvement of methods for estimation of residual life of welded joints in durable structures. Ibid., 10/11, 107–116.
3. Mirkin, I.L. (1958) On atomic mechanism of ageing of complex adding alloys. Transact, of Seminar of AS Ukr. SSR on Heat-Resistant Materials, 3, 3–26.
4. Rozenberg, V.M. (1967) Creep of metal. Moscow: Metallurgiya.
5. Geguzin, Ya.E. (1962) Macrodefects in metals. Moscow: Metallurgizdat.
6. Dmitrik, V.V. (2000) Structure of welded joints from lowalloyed heat-resistant Cr-Mo-V pearlitic steels. The Paton Welding J., 4, 26–29.
7. Antikajn, P.A. (1984) Safety control of boilers, vessels and pipelines after termination of designed service life. Teploe- nergetika, 2, 74–75.
8. Khromchenko, F.A. (2002) Life of welded joints of steam supply lines. Moscow: Mashinostroenie.
9. Borggreen, K., Huntley, P. (1984) Correction to the constant stress augmented temperature extrapolation method due to oxidation of the subsize creep specimens. In: Proc, of 2nd Int. Conf, on Creep and Fracture of Engineering Materials and Structures (Swansea, April 1–6, 1984). Swansea.
10. Dmitrik, V.V., Pashchenko, A.N. (2003) Decrease in structural heterogeneity of incomplete refining region of the HAZ of welded joints in pearlitic steels. The Paton Welding J., 1, 14–18.
11. Zemzin, V.N., Shron, R.Z. (1978) Heat treatment and properties of welded joints. Leningrad: Mashinostroenie.
12. Anokhov, A.E., Alekhova, LA. (1982) Damage accumulation in welded joints of 12KMMF steel steam supply line in creep process. Svarochn. Proizvodstvo, 9, 34–35.
13. Berezina, T.G. (1986) Structural method of determination of residual life of steam supply line parts being in long-term service. Teploenergetika, 3, 53–56.
14. Kumanin, V.I., Kovalyova, L.A., Alekseev, S.V. (1988) Life of metal in creep conditions. Moscow: Metallurgiya.
15. Berezina, T.G., Shklyarov, M.I., Shtromberg, Yu.Yu. (1992) Evaluation of life of power equipment parts in creep conditions taking into account the structural factor. Teploenergetika, 2, 2–5.
16. Zlepko, V.F., Perevezentseva, T.V., Novikov, S.V. (1991) Some specifics of structural state of metal of centrifugal-cast steam supply line pipes of 15KhlMlF steel. Elektrich. Stantsii, 3, 40-43.
17. Barret, Ch.S., Massalsky, T.B. (1984) Structure of metals. Moscow: Metallurgiya.
18. Gulyaev, A.P. (1978) Metals science. Moscow: Metallurgiya.
19. (1972) Metallography of iron. Vol. 1: Principles of metallography. Ed. by F.N. Tavadze. Moscow: Metallurgiya.
20. Pigrova, G.D. (2003) Effect of long-term service on carbide phases in Cr-Mo-V steels. Metallovedenie i Term. Obrab. Metallov, 3, 6–9.
21. (1976) Tables of physical magnitudes. Refer. Book. Ed. by K. Kikoin. Moscow: Atomizdat.

Suggested Citation

V.V. Dmitrik, A.I. Konyk (2005) On concept of pore initiation in welded joints under low-temperature creep. The Paton Welding J., 07, 24-27.