The effect of parameters of the asymmetric and modulated currents on the length of oxide film inclusions in the welds and porosity of the joints in alloys AMg6, 1420 and 1460 produced by a pulsed-arc TIG welding is considered. The use of the asymmetric current allows a decrease of 3 times in the relative length of the oxide film inclusions in the AMg6 alloy welds and reduces the probability of formation of whisker inclusions in the welds. Efficient degassing of the molten pool metal is achieved in the case of using the modulated current with a modulation frequency of 5 Hz.
Keywords: pulsed arc, asymmetric current, modulated current, non-consumable electrode, aluminium alloys, inclusions of oxide film, pores

References

1. Moiseenko, I.G., Stolbov, V.I., Turchenko, M.A. (1968) Oxide inclusions in welding alloy AMg6. Svarochnoye Proizvodstvo, 5, 23 - 24.
2. Moiseenko, I.G., Lukashin, N.V. (1969) Towards the problem of improvement the air-tightness of alloy AMg6 welded vessels. Ibid., 8, 31 - 32.
3. Lukianov, V.F., Fomin, V.N., Moiseenko, V.P. et al. (1970) Effect of oxide inclusions on strength of welded joints of AMg6 alloy pressure vessels. Ibid., 6, 24.
4. Ishchenko, A.Ya., Chayun, A.G., Beletsky, V.M. et al. (1977) Peculiarities of fusion welding of aluminium alloy 01420. Avtomaticheskaya Svarka, 3, 38 - 41.
5. Barabokhin, N.S., Bushuev, Yu.G., Shulgina, E.V. et al. (1999) Technological peculiarities of welding high-strength aluminium allov 1460. Svarochnoye’ Proizvodstvo, 11, 12 - 14.
6. Shiryaeva, N.V., Ovchinnikov, V.V., Gabidullin, R.M. (1987) Pore formation in welding alloy of aluminium-magncsium-lithium system. Avtomaticheskaya Svarka, 3, 16 - 18.
7. Oboturov, V.I., Tolkachev, Yu.N. (1973) Some peculiarities of formation and destroying of oxide films in argon-arc welding of aluminium allovs. Svarochnoye Proizvodstvo, 11,22 - 24.
8. Sushkov, V.N., Skachkov, Yu.N., Novikov, O.M. et al. (1975) Susceptibility of light alloys to the oxide inclusions formation during welding. Ibid., 5, 23 - 24.
9. Chayun, A.G., Syrovatka, V.V., Matyash, V.I. (1981) Arc welding of aluminium alloy 01420 using EMP. Avtomaticheskaya Svarka, 6, 19-21.
10. Ishchenko, A.Ya., Chayun, A.G., Ilyushenko, R.V. (1985) Weldability and technology of arc welding of alloy of aluminium-magnesium-lithium system. Ibid., 10, 47 - 49.
11. Poklyatsky, A.G., Ishchenko, A.Ya., Bessonov, A.S. et al. (1991) Prevention of oxide film formation in welds during a pulsed-arc welding aluminium alloys. Ibid., 7, 43 - 47.
12. Maruo, H., Hirata, Yo., Makino, H. (1989) Rectangular wave AC TIG arc welding of aluminium allov. Q. J. of Л VS, 1,63 - 69.
13. Ishchenko, A.Ya., Poklyatsky, A.G., Yavorskaya, M.R. (1989) Prevention of oxide film inclusions in welds in argon-arc welding of aluminium alloys. Avtomaticheskaya Svarka, 6, 38 – 41.