The Paton Welding Journal, 2005, #11, 29-33 pages

Repair of railway wagon wheels by cladding with preliminary annealing of roll surfaces

V.V. Matveev

Closed Joints Stock Company «Viltrans», Kiev, Ukraine

Abstract
The set of technological problems to be addressed in the process of repair of railway wheels by cladding is considered. The technology is offered for high-productivity multi-electrode cladding of wheels after annealing of the roll surfaces
Keywords: repair, wagon wheels, defects on roll surface, high-frequency heating, HFC annealing, multi-electrode cladding, microstructure

References

1. Asnis, A.E., Gutman, L.M., Stepenko, V.P. et al. (1958) Submerged-arc welding in repair of locomotives. Moscow: Transzheldorizdat.
2. (2001) ESAB delivers engineered automatic welding station to Ghana in Africa for build-up welding of worn railway wheels. Svetsaren, 1, 20−21.
3. Pavlov, N.V., Kozubenko, I.D., Byzova, I.E. et al. (1993) Surfacing of flanges of railway wheelsets. ZhD Transport, 7, 37−40.
4. (1977) TsV/3429: Instructions for examination, inspection, repair and formation of railway wheelsets. Moscow: Transport.
5. Tsyurenko, V.N. (2002) Operational reliability of freight car wheelsets. ZhD Transport, 3, 24−28.
6. Uzlov, I.G. (1985) Wheel steel. Kiev: Tekhnika.
7. Matveev, V.V. (2005) Cladding of wagon wheel flanges after annealing of the roll surfaces at wagon repair factories of Ukraine. The Paton Welding J., 6, 36−41.
8. Matveev, V.V. Method for restoring of roll surfaces of railway transport wheels. Pat. 44373 Ukraine. Publ. 15.02.02.
9. Vologdin, V.P. (1974) Surface induction hardening. Mos¬cow; Oborongiz.
10. Melikov, V.V. (1988) Multi-electrode surfacing. Moscow: Mashinostroenie.
11. Emelianov, N.P. (1962) Multi-electrode submerged-arc and electroslag surfacing. In: Transact, of All-Union Res. Institute of Railway Transport. Issue 239.
12. Matveev, V.V., Olshevsky, V.I. Method for restoration of profiles of railway transport wheel rim surfaces. Pat. 61794 Ukraine. Publ. 15.07.05.

Suggested Citation

V.V Matveev (2005) Repair of railway wagon wheels by cladding with preliminary annealing of roll surfaces. The Paton Welding J., 11, 29-33.