TPWJ, 2010, #12, 5-8 pages
RISK OF FORMATION OF CARBIDES AND a-PHASE IN WELDING OF HIGH-ALLOY CHROME-NICKEL STEELS
Journal The Paton Welding Journal
Publisher International Association «Welding»
ISSN 0957-798X (print)
Issue № 12, 2010 (December)
Pages 5-8
Authors
V.I. MAKHNENKO1, S.S. KOZLITINA1, L.I. DZYUBAK1 and V.P. KRAVETS2
1E.O. Paton Electric Welding Institute, NASU, Kiev, Ukraine
2Rivnenskaya NPP, Kuznetsovsk, Ukraine
Abstract
The possibility is considered of using calculation methods to predict the risk of formation of the s-phase in the HAZ metal of chrome-nickel steels at a carbon content of about 0.08 % and higher. It is shown that the use of temperature-time constitutional diagrams for steel of a corresponding composition, combined with temperature cycles at points in the HAZ metal, allows predicting the degree of sensitization of the corresponding HAZ region under different welding conditions.
Keywords: arc welding, chrome-nickel steels, welded joints, sensitization, s-phase, intergranular cracks, stress corrosion, temperature-time diagram
Received: ??.??.??
Published: 28.12.10
References
1. (1998) Welding handbook. Materials and applications. Pt 2. Miami: AWS.
2. Elter, J.W., Palmer, T.A., Specht, E.D. (2006) Synchrotron based observations of sigma phase formation and dissolution in DSS. Ed. by H. Cerjak. In: Mathematical modeling of weld phenomena, 297-315.
3. Hell, E.O., Alqie, S.H. (1966) The sigma phase. Metallurgical Rev., 11, 61-68.
4. (1986) Metallurgy and technology of welding of titanium and its alloys. Ed. by V.N. Zamkov. Kiev: Naukova Dumka.
5. Zubchenko, A.S., Kharina, I.L., Runov, A.E. et al. (2000) Corrosion-mechanical strength of welded piping of austenitic steels of RBMK reactors. The Paton Welding J., 9/10, 45-53.
6. Makhnenko, V.I. (2006) Safety service life of welded joints and assemblies of current structures. Kiev: Naukova Dumka.