Print

2015 №07 (01) DOI of Article
10.15407/tpwj2015.07.02
2015 №07 (03)

The Paton Welding Journal 2015 #07
The Paton Welding Journal, 2015, #7, 10-15 pages
 

Peculiarities of degradation of metal in welded joints of steam pipelines

V.V. Dmitrik1, O.V. Sobol1, M.A. Pogrebnoj1 And T.A. Syrenko2


1National Technical University «Kharkov Polytechnic Institute». 21 Frunze Str., 61002, Kharkov, Ukraine. E-mail: svarka126@ukr.net
2Kharkov Machine-Building College. 79 Plekhanovskaya Str., 61068, Kharkov, Ukraine
 
 
Abstract
Extension of life of steam pipelines, operated under creep conditions, determines the necessity of evaluation of their damageability and in many respects depends on carbide transformations in metal. The work considers peculiarities of diffusion and structure of carbide phases in metal of welded joints of pearlite steels after long-term operation. It is determined that concentration of coagulating carbide phases (M23C6, M7C3 etc.) at the boundaries of a-phase grains promotes for nucleation of creep pores and fatigue cracks, that causes brittle fracture of metal of welded joints. 18 Ref., 8 Figures.
 
Keywords: team pipeline welded joints, carbide phases, creep pores, fatigue cracks, damageability, operation life
 
 
Received:                18.02.15
Published:               13.10.15
 
 
References
  1. Gladshtejn, V.I. (2007) Influence of running up to 350,000 hours on service characteristics and structure of cast body parts of turbines and fittings. Metallovedenie i Term. Obrab. Metallov, 4, 24-32.
  2. Khromchenko, F.A., Kalugin, R.N. (2004) Calculation-experimental method for evaluation of residual life of welded joints in steam pipelines. The Paton Welding J., 5, 6-11.
  3. Rezinskaya, V.F., Grin, E.A. (2013) Current problems of safety assurance of heat-mechanic equipment in prolongation of its service life. Teploenergetika, 1, 17-24.
  4. Dmitrik, V.V., Bartash, S.N. (2014) Peculiarities of degradation of metal of welded joints in steam pipelines of heat power plants. The Paton Welding J., 6/7, 29-30. https://doi.org/10.15407/tpwj2014.06.05
  5. Sirotyuk, A.M., Kapty, O.V., Dmitrakh, I.M. et al. (2013) Expert system for evaluation of structural element fracture of pipelines of heat-and-power engineering system. Metody ta Prylady Kontr. Yakosti, 2, 126-136.
  6. Trubachyov, V.M., Kamenskaya, N.I. (2012) Methods for evaluation of microdamageability of metal of steam pipelines in long-term operation of thermal power plant. Metallovedenie i Term. Obrab. Metallov, 8, 49-54.
  7. Danyushevsky, I.A., Kupry, E.B., Malkin, M.R. et al. (2008) Evaluation of residual life taking into account microdamageability. Teploenergetika, 2, 12-17.
  8. Dmitrik, V.V., Syrenko, T.A. (2012) To the mechanism of diffusion of chromium and molybdenum in the metal of welded joints of steam pipelines. The Paton Welding J., 10, 20-24.
  9. Bokshtejn, B.S. (1978) Diffusion in metals. Moscow: Metallurgiya.
  10. Gottshtajn, G. (2011) Physico-chemical principles of materials science. Moscow: BINOM.
  11. Dmitrik, V.V., Baumer, V.N. (2007) Carbide phases and damageability of welded joints in long-term service. Metallofizika, Nov. Tekhnologii, 7, 937-947.
  12. Dmitrik, V.V., Syrenko, T.A. (2010) Specifics of temper brittleness of steam pipeline welded joints. Energosberezhenie. Energetika. Energoaudit, 4, 29-35.
  13. Lashko, N.F., Zaslavskaya, L.V., Kozlova, M.N. et al. (1978) Physico-chemical and phase analysis of steels and alloys. Moscow: Metallurgiya.
  14. Lanskaya, K.A. (1969) Heat-resistant steels. Moscow: Metallurgiya.
  15. Rafaja, D., Lengauer, W., Ettmayer, P. et al. (1998) Rietveld analysis of the ordering in V8C7. J. Alloys and Compounds, 3, 60-62. https://doi.org/10.1016/S0925-8388(97)00489-1
  16. Fruchart, D., Chaudouet, P., Fruchart, R. (1984) Etudes structurales de composes de type cementite: effet de l'hydrogene sur Fe3C suivi par diffraction electronique spectrometrie moessbauer sur FeCo2B et Co3B dopes au 57Fe. J. Solid State Chemistry, 51, 246-252. https://doi.org/10.1016/0022-4596(84)90340-2
  17. Rodriguez-Carvajal, J., Rossnel, T. (1988) Full Prof. 98 and Win PLOTR: New Windows 95/NT applications for diffraction. Commission for Powder Diffraction, International Union of Crystallography Newsletter 20, 5-8, 159.
  18. Dmitrik, V.V., Tsaryuk, A.K., Konyk, A.I. (2008) Carbide phases and damageability of welded joints of steam pipelines under creep conditions. The Paton Welding J., 3, 28-32.

Suggested Citation

V.V. Dmitrik, O.V. Sobol, M.A. Pogrebnoj And T.A. Syrenko (2015) Peculiarities of degradation of metal in welded joints of steam pipelines. The Paton Welding J., 07, 10-15.