The Paton Welding Journal, 2002, #10, 44-46 pages

Peculiarities of deoxidation of the weld pool metal in plasma surfacing with composite materials

A.I. Bely, A.P. Zhudra, V.I. Dzykovich

E.O. Paton Electric Welding Institute of the NASU 11 Kazymyr Malevych Str., 03150, Kyiv, Ukraine.

Abstract
Experiments on deoxidation of matrix of granular tungsten carbide based composite alloys in plasma surfacing, transfer of aluminium to the deposited metal and its effect on arrangement of reinforcing particles (WC-W2C) in the wear-resistant layer are described.
Keywords: plasma surfacing, filler material, composite alloy matrix, reinforcing particles, deoxidation

References

1. Bely, A.I. The process of plasma surfacing using composite alloys. Author’s cert. 1622097, Int. Cl. В 23 К 9'04. Publ. 23.01.91.
2. Vojtovich, R.F., Pugach, E.A. (1975) nigh-temperature oxidation of carbides of group IV-VI metals. In: High-temperature carbides. Kyiv: Naukova Dumka.
3. Zhudra, A.P. (1980) Study and development of materials designed for surfacing with composite abrasive wear-resistant alloys. Syn. of Thesis for Cand. of Techn. Sci. Degree. Kyiv
4. Pokhodnya, I.K., Suptel, A.M., Shlepakov, V.N. (1972) Flux-cored wire welding. Kyiv: Naukova Dumka.
5. Yuzvenko, Yu.A., Kirilyuk, G.A. (1973) Flux-cored wire surfacing. Kyiv: Naukova Dumka.
6. Potapievsky, A.G. (1974) Shielded-gas metal-arc welding. Moscow: Mashinostroenie.
7. Bagryansky, K.V., Dobrotina, Z.A., Khrenov, K.K. (1976) Theory of welding processes. Kyiv: Vyshcha Shkola.
8. Gasik, L.N., Ignatiev, V.S., Gasik, M.I. (1975) Structure and quality of commercial ferroalloys and master alloys. Kyiv: Tekhnika.

Suggested Citation

A.I. Bely, A.P. Zhudra, V.I. Dzykovich (2002) Peculiarities of deoxidation of the weld pool metal in plasma surfacing with composite materials. The Paton Welding J., 10, 44-46.