The Paton Welding Journal, 2011, #8, 46-48 pages
DEVELOPMENT OF THE METHODS FOR ELIMINATION OF DEFORMATION OF CRANKSHAFTS IN WIDE-LAYER HARDFACING
S.Yu. KRIVCHIKOV
E.O. Paton Electric Welding Institute, NASU, Kiev, Ukraine
Abstract
Methods were developed for elimination of deformation of crankshafts of car engines caused by wide-layer hardfacing at their reconditioning. It is established that an effective method to eliminate deformations is preheating of hardfaced bearings and (or) application of axial tensile load to the crankshaft during hardfacing.
Keywords: arc wide-layer hardfacing, crankshafts, deformation, measures of elimination
Received: ??.??.??
Published: 28.08.11
References
1. Zhudra, A.P., Krivchikov, S.Yu., Petrov, V.V. (2010) Technology for wide-layer hardfacing of crankshafts. The Paton Welding J., 2, 32-35.
2. Krivchikov, S.Yu., Zhudra, A.P., Petrov, V.V. et al. (1998) Thermal cycle of wide-layer hardfacing of cylindrical cast iron parts with self-shielded flux-cored wire. Avtomatich. Svarka, 4, 49-50.
3. Gretsky, Yu.Ya., Novikova, D.P., Kroshina, G.M. (1986) Influence of thermal cycle on resistance of cast irons to cracking in welding without preheating. Ibid., 4, 1-4, 13.
Suggested Citation
S.Yu. KRIVCHIKOV (2011) DEVELOPMENT OF THE METHODS FOR ELIMINATION OF DEFORMATION OF CRANKSHAFTS IN WIDE-LAYER HARDFACING.
The Paton Welding J., 08, 46-48.