The Paton Welding Journal, 2024, #4, 18-22 pages
Detonation coatings produced by spraying of alloyed powders based on Fe–Al intermetallics
N.V. Vigilianska, T.V. Tsymbalista, A.I. Kildii, C.V. Iantsevitch, Z.G. Ipatova, M.A. Vasylkivska
E.O. Paton Electric Welding Institute of the NASU.
11 Kazymyr Malevych Str., 03150, Kyiv, Ukraine. E-mail: pewinataliya@gmail.com
Abstract
The research results on the structure, phase composition, and properties of detonation coatings produced by spraying
a mechanical mixture of Fe powders and AlMg and TiAl alloys, as well as composite powders of the same composition
synthesized by the mechanochemical method, are presented. It was found that in the coatings produced with the use of
mechanical mixtures of powders, the synthesis of intermetallic compounds does not occur and the coatings consist of initial
components and their oxides. Therefore, it is advisable to use powders produced by the method of mechanochemical synthesis as
spray materials. This results in the formation of coatings, in which the main phase is the Fe-Al intermetallic compound. Coatings
of the Fe-AlMg and Fe-TiAl systems, produced by spraying of composite powders, are characterized by a dense lamellar
structure consisting of alternating layers of metal and oxide components. The coatings exhibit high oxidation resistance in the
temperature range of 700-800 °C, comparable to the oxidation resistance of cast iron-aluminium alloys, and allow increasing
the oxidation resistance of carbon steels by 6–20 times. The corrosion resistance of Fe-AlMg and Fe-TiAl detonation coatings
in a 3% NaCl solution exceeds the corrosion resistance of uncoated carbon steel by 13.3 and 28.0 times, respectively. The
obtained results allow recommending to use the developed coatings for protection of parts operating in aggressive environments
at temperatures of up to 800 °C. 19 Ref., 2 Tabl., 3 Fig.
Keywords: intermetallic compounds of the Fe-Al system, mechanochemical synthesis, composite powders, detonation spraying,
coating, oxidation resistance, corrosion resistance
Received: 30.11.2023
Received in revised form: 16.02.2024
Accepted: 02.05.2024
References
1. Deevi, S.C., Sikka, V.K. (1996) Nickel and iron aluminides: an overview on properties, processing, and applications. Intermetallics, 4(5), 357-375.
https://doi.org/10.1016/0966-9795(95)00056-92. Stoloff, N.S. (1998) Iron aluminides: present status and future prospects. Materials Sci. and Engin.: A, 258(1-2), 1-14.
https://doi.org/10.1016/S0921-5093(98)00909-53. Palm, M., Stein, F., Dehm, G. (2019) Iron Aluminides. Annual Review of Materials Research, 49(1).
https://doi.org/10.1146/annurev-matsci-070218-1259114. Zamanzade, M., Barnoush, A., Motz, C. (2016) A Review on the Properties of Iron Aluminide Intermetallics. Crystals, 6(1), 10.
https://doi.org/10.3390/cryst60100105. Senderowski, C., Chodala, M., Bojar, Z. (2015) Corrosion Behavior of Detonation Gun Sprayed Fe-Al Type Intermetallic Coating. Materials, 8(3), 1108-1123.
https://doi.org/10.3390/ma80311086. Peng, J., Moszner, F., Rechmann, J. et al. (2019) Influence of Al Content and Pre-oxidation on the Aqueous Corrosion Resistance of Binary Fe-Al Alloys in Sulphuric Acid. Corrosion Science, 149, 123-132.
https://doi.org/10.1016/j.corsci.2018.12.0407. Baligidad, R.G., Prasad, V.V. Satya, Rao, A. Sambasiva (2007) Effect of Ti, W, Mn, Mo and Si on microstructure and mechanical properties of high carbon Fe-10·5 wt-%Al alloy. Materials Science and Technology, 23(5), 613-619.
https://doi.org/10.1179/174328407X1586318. Stein, F., Schneider, A., Frommeyer, G. (2003) Flow stress anomaly and order-disorder transitions in Fe3Al-based Fe- Al-Ti-X alloys with X=V, Cr, Nb, or Mo. Intermetallics, 11(1), 71-82.
https://doi.org/10.1016/S0966-9795(02)00187-59. Zamanzade, M., Vehoff, H., Barnoush, A. (2013) Effect of chromium on elastic and plastic deformation of Fe3Al intermetallics. Intermetallics, 41, 28-34.
https://doi.org/10.1016/j.intermet.2013.04.01310. Krein, R., Schneider, A., Sauthoff, G., Frommeyer, G. (2007) Microstructure and mechanical properties of Fe3Al-based alloys with strengthening boride precipitates. Intermetallics, 15(9), 1172-1182.
https://doi.org/10.1016/j.intermet.2007.02.00511. Deevi, S.C. (2020) Advanced Intermetallic Iron Aluminide Coatings for High Temperature Applications. Progress in Materials Science, 100769.
https://doi.org/10.1016/j.pmatsci.2020.10076912. Cinca, N., Guilemany, J. M. (2012) Thermal spraying of transition metal aluminides: An overview. Intermetallics, 24, 60-72.
https://doi.org/10.1016/j.intermet.2012.01.02013. Borisov, Yu.S., Borisova, A.L., Burlachenko, A.N. et al. (2017) Structure and properties of alloyed powders based on Fe3Al intermetallic for thermal spraying produced using mechanochemical synthesis method. The Paton Welding J., 9, 33-39.
https://doi.org/10.15407/tpwj2017.09.0614. Borisov, Yu.S., Borisova, A.L., Astakhov, E.A. et al. (2017) Detonation coatings of intermetallic powders of Fe-Al system produced using mechanical alloying. The Paton Welding J., 4, 23-29.
https://doi.org/10.15407/tpwj2017.04.0515. metals and alloys. Lviv, SPOLOM [in Ukrainian].
16. Sakhnenko, M.D., Ved, M.V., Yaroshok, T.P. (2005) Basics of the theory of corrosion and protection of metals. Kharkiv, NTU KhPI [in Ukrainian].
17. Haušild, P., Karlík, M., Skiba, T. et al. (2012) High Temperature Oxidation of Spark Plasma Sintered and Thermally Sprayed FeAl-Based Iron Aluminides. Acta Physica Polonica A, 122, 465-468. Doi: 10.12693/APHYSPOLA.122.465 18. Marx, V., Palm, M. (2016) Oxidation of Fe-Al Alloys (5-40 at.% Al) at 700 and 900 ºC. Materials Science Forum, 879, 1245-1250.
https://doi.org/10.4028/www.scientific.net/MSF.879.124519. Vihilianska, N.V., Gryshchenko, O.P., Iantsevych, K.V. et al. (2022) Corrosion resistance of plasma coatings based on composite powders with FeAl intermetallic. The Paton Welding J., 12, 35-39.
https://doi.org/10.37434/tpwj2022.12.05
Suggested Citation
N.V. Vigilianska, T.V. Tsymbalista, A.I. Kildii, C.V. Iantsevitch, Z.G. Ipatova, M.A. Vasylkivska (2024) Detonation coatings produced by spraying of alloyed powders based on Fe–Al intermetallics.
The Paton Welding J., 04, 18-22.