The Paton Welding Journal, 2005, #8, 44-49 pages

Laser-arc and laser-plasma welding and coating technologies

V.D. Shelyagin, I.V. Krivtsun, Yu.S. Borisov, V.Yu. Khaskin, T.N. Nabok, A.V. Siora, A.V. Bernatsky, S.G. Vojnarovich, A.N. Kislitsa, T.N. Nedej

E.O. Paton Electric Welding Institute of the NASU. 11 Kazymyr Malevych Str., 03150, Kyiv, Ukraine.

Abstract
Peculiarities of processes occurring in the case of combined utilisation of laser beam and consumable-electrode arc or plasma jet are considered. Fundamentally new approaches have been developed for one- and multipass hybrid laser-arc welding, as well as combined and hybrid laser-microplasma deposition of coatings (including diamond and diamond-like thin coatings). Advantages of the new hybrid (combined) processes are shown in comparison with the available laser and arc ones.
Keywords: laser welding, filler wire, arc, consumable electrode, hybrid process, steels, aluminium alloys, large thickness, multipass welding, conditions, heat input, microplasma, combined process, surface alloying, coating, diamond and diamondlike coatings, metallography, structures, properties

References

1. (1974) Technology of electric fusion welding of metals and alloys. Ed. by B.E. Paton. Moscow: Mashinostroenie.
2. Seyffarth, P., Krivtsun, I.V. (2002) Laser-arc processes and their applications in welding and material treatment. Vol. 1. London: Taylor and Fransis Books.
3. Shelyagin, V.D., Khaskin, V.Yu. (2002) Tendencies in development of laser-arc welding (Review). The Paton Weldingj., 6, 25–28.
4. Shelyagin, V.D., Khaskin, V.Yu., Garashchuk, V.P. et al. (2002) Hybrid CO2-laser and CO2 consumable-arc wielding. Ibid., 10, 35–37.
5. Garashchuk, V.P., Shelyagin, V.D., Nazarenko, O.K. et al. (1997) Technological 10 kW CO2-laser LT 104. Avtomatich. Svarka, 1, 36–39.
6. Gulyaev, A.P. (1963) Metals science. Moscow: Oborongiz.
7. Nazarenko, O.K., Kajdalov, A.A., Kovbasenko, S.N. et al. (1987) Electron beam welding. Ed. by B.E. Paton. Kiev: Naukova Dumka.
8. Semyonov, S.E., Mandelberg, S.L., Goncharenko, L.V. (1989) The optimal level of impact toughness of gas pipe weld metal. Avtomatich. Svarka, 11, 55–57.
9. Coddet, C., Montaron, G., Marchione, T. et al. (1998) Surface preparation and thermal spray in a single step: the PROTAL process. In: Proc, of 15th ITSC (Nice, France). Vol. 2.
10. Li, R., Shi, H., Yan, Z. et al. (1991) Deposition of diamond film by DC arc plasma CVD. In: Proc, of 2nd Plasma-Technique Symposium (Lucerne, Switzerland). Vol. 1.
11. Lugscheider, E., Muller, U., Deuerler, F. et al. (1993) Synthesis of crystalline diamond coatings by the DC-plasma jet CVD process. In: Proc. ofITSC (Duesseldorf, Germany).
12. Lugscheider, E., Weber, T., Schlump, W. (1991) General study assciated with diamond syrlliesis by vacuum pl;isrn;i spraying or DC arc plasma vapour deposition. In: Proc, of ITSC (Pittsburg, USA).
13. Borisov, Yu.S., Vojnarovich, S.G., Bobrik, V.G. et al. (2000) Microplasma spraying of bioceramic coatings. Avtomatich. Svarka, 12, 63–67.

Suggested Citation

V.D. Shelyagin, I.V. Krivtsun, Yu.S. Borisov, V.Yu. Khaskin, T.N. Nabok, A.V. Siora, A.V. Bernatsky, S.G. Vojnarovich, A.N. Kislitsa, T.N. Nedej (2005) Laser-arc and laser-plasma welding and coating technologies. The Paton Welding J., 08, 44-49.