The Paton Welding Journal, 2003, #5, 38-43 pages
Producing welded joints equivalent in strength on quenching steels without preheating and heat treatment
A.T. Nazarchuk, V.V. Snisar, E.L. Demchenko
E.O. Paton Electric Welding Institute of the NASU
11 Kazymyr Malevych Str., 03150, Kyiv, Ukraine.
Abstract
The paper deals with the possibility of producing equivalent joints on high-strength quenching steels by arc welding without preheating and heat treatment. Good prospects for application of austenitic-martensitic consumables in welding of high-strength steels without preheating and heat treatment with the level of weld metal strength of 1150−1200 MPa.
Keywords: welding, quenching steels, high-strength steels, multilayer welds, high-strength welds, welded joints, delayed fracture, process strength, cold cracks
References
1. (1962) Technology of electric fusion welding. Ed. bv B.E. Paton. Moscow-Kyiv: Mashgiz.
2. (1974) Technology of electric fusion welding of metals and alloys. Ed. by B.E. Paton. Moscow: Mashinostroenie.
3. Makara, A.M. (1963) Investigation of the problems of technology and metals science in welding alloyed structural steels. Kviv: PWI.
4. Makarov, E.L. (1981) Cold cracks in welding. Moscow: Mashinostroenie.
5. Shorshorov, M.Kh. (1965) Metals science of steel and titanium welding. Moscow: Nauka.
6. Kasatkin, S.B., Mikhoduj, L.I., Gordonny, V.G. (1996) Procedural approaches to integrated investigation of delayed and brittle fracture in high-strength low-alloy steels. Aotomatich. Svarka, 2, 58-60.
7. Kasatkin, B.S., Brednev, V.l. (1985) Peculiarities of cold cracking mechanism in welded joints of high-strength steels. Ibid., 8, 1−6, 18.
8. Kasatkin, B.S., Brednev, y.L, Tsaryuk, A.K. et al. (1993) Estimation of resistance of 15Kh2MFA steel welded joints to cold cracking. Ibid., 5, 3−7.
9. Tsaryuk, A.K., Brednev, V.l. (1996) Problems of cold 23. cracking prevention. Ibid., i, 36−40.
10. Tsaryuk, A.K., Brednev, V.l. (1998) On the nature of cold cracking in welding of quenching steels. Ibid., 10, 9-13.
11. Mikhoduj, E.L, Poznyakov, V.D., Yushchenko, A.K. (2000) Resistance of 12KhGN2MFDRA steel welded joints to a delaved fracture. The Paton Welding J., 11, 4−10.
12. Musiyachenko, V.F., Kasatkin, S.B. (1985) Distribution of hydrogen in alloyed steel welded joint and its influence on 25. cold cracking (Review). Avtomatich. Svarka, 9, 3-8.
13. Pokhodnya, I.K., Shvachko, V.l. (1997) Physical nature of hvdrogen induced cold cracks in welded joints of structural steels. Ibid., 5, 3−12.
14. Pokhodnya, I.K., Stepanyuk, S.N., Shvachko, V.l. (2000) Role of temperature in hydrogen-induced cracking of structural steels and welded joints. The Paton Welding J., 2, 2−7.
15. Makara, A.M., Gordonny, V.G., Dibets, A.T. et al. (1971) Cold cracks in low-alloy high-strength welds. Avtomatich. Svarka, 11, 1−4.
16. Nazarchuk, A.T., Sterenbogen, Yu.A., Kosyakov, V.P. (1984) Procedure of evaluation of weld metal susceptibility to formation of transverse cracks. Ibid., 12, 7−10.
17. Nazarchuk, A.T., Sverdel, l.P. (1994) Resistance of quenching steel joints with multilaver welds to crack formation. Ibid., 1, 15−19.
18. Nazarchuk, A.T., Sterenbogen, Yu.A. (1984) About optimisation of arc welding process bv efficient groove filling. Ibid., 11, 46−49.
19. Nazarchuk, A.T. (1994) Control of weld metal solidification and thermodeformational cvcle in automatic arc welding. Ibid., 5/6, 3−9.
20. Nazarchuk, A.T. (1997) Influence of portion-discrete weld formation on the thermal cvcle of fusion arc welding. Ibid., 5, 13−17.
21. Nazarchuk, A.T., Sverdel, l.P., Nikulin, V.A. (1995) Twinarc welding without phereating of banding of 34KhNlM and 34KhN3M steels to discs of large-sized toothed wheels of St.3 steel. Ibid., 1, 30−34.
22. Nazarchuk, A.T. (1992) Examination of the influence of the proportion of layers with different properties on mechanical characteristics of two-laver steel samples. Ibid., 7, 27−29, 32.
23. Gotalsky, Yu.N., Snisar, V.V., Kuporev, A.L. et al. Method of arc welding of quenching steels. USSR author’s cert. 880671. Int. Cl. B 23 K 28/00. Publ. 15.11.81.
24. Lipodaev, V.N., Gotalsky, Yu.N., Snisar, V.V. et al. Electrode for welding of low- and medium-alloy high-strength quenching steels without preheating and heat treatment. USSR author’s cert. 1689007. Int. Cl. B 23 K 35/36. Publ. 08.07.91.
25. Demchenko, E.L., Lyakhovaya, I.V., Snisar, V.V. et al. Electrode for welding of high-strength steels. USSR author’s cert. 1785860. lilt. Cl. B 23 K 35/365. Publ. 08.09.92.
26. Gotalsky, Yu.N., Snisar, V.V., Demchenko, E.L. et al. Welding of high-strength steels with the yield point above 800 MPa without preheating and heat treatment. Avtomatich. Svarka, 10, 38−40.
27. Snisar, V.V., Demchenko, E.L., Ivanchenko, E.V. (2000) Challenging technologies for high-strength steel welding without preheating and heat treatment. The Paton Welding J., 11, 37−40.
28. Demchenko, E.L., Snisar, V.V., Lipodaev, V.N. et al. Means of lowering the hvdrogen content in weld metal of 03Khf 2N8M2GST type during arc welding. Avtomatich. Svarka, 10, 23−27.
29. Snisar, V.V., Demchenko, E.L., Gajvoronsky, A.A. (1993) Influence of weld structure on HAZ properties in 30Kh2N2M steel welded joints. Ibid., 9, 43−45.
Suggested Citation
A.T. Nazarchuk,
V.V. Snisar,
E.L. Demchenko (2003) Producing welded joints equivalent in strength on quenching steels without preheating and heat treatment.
The Paton Welding J., 05, 38-43.