Effect of zirconia on properties of slag in flux-cored wire submerged-arc surfacing using flux AN-348A

V.E. Sokolsky1, A.S. Roik1, V.P. Kazimirov1, I.I. Ryabtsev2, D.D. Mishchenko2, I.A. Ryabtsev2, A.S. Kotelchuk2, V.S. Tokarev2

1Taras Shevchenko Kiev National University, Kiev, Ukraine
2E.O. Paton Electric Welding Institute of the NASU. 11 Kazymyr Malevych Str., 03150, Kyiv, Ukraine.

Abstract
Effect of zirconia on slag properties in submerged-arc surfacing using low-alloy flux-cored wire PP-Np-20KhGS and flux AN-348A was investigated. It is established that, when depositing the first layers, zirconia is contained in the surface layer of the slag crust adjacent to the deposited metal in the form of individual inclusions of predominantly monoclinic shape. Formation of zirconia induces substantial microstresses in the slag crust and leads to its cracking, thus preventing chemical bonding of the crust and deposited metal through an interlayer of oxides and improving detachability of the slag crust.
Keywords: arc surfacing, submerged-arc surfacing, fluxcored wire, zirconia, detachability of slag crust, X-ray examinations

References

1. Frumin, I.I. (1961) Automatic arc surfacing. Kharkov: Metallurgizdat.
2. Podgaetsky, V.V. (1952) Some peculiarities of metallurgical processes in submerged-arc welding of steel: Syn. Of Thesis for Cand. of Techn. Sci. Degree. Kiev.
3. Pokhodnya, I.K., Yavdoshchin, I.R., Karmanov, V.I. et al. (1974) Mechanism of cohesion between slag crust and weld surface. Avtomatich. Svarka, 5, 5–9.
4. Pokhodnya, I.K., Karmanov, V.I., Vojtkevich, V.G. (1976) Investigation of peculiarities of cohesion mechanism between slag crust and weld metal alloyed with titanium and vanadium. Ibid., 6, 1–4.
5. Pokhodnya, I.K., Demchenko, L.I., Yavdoshchin, I.P. et al. (1977) Kinetics of formation of intermediate layer between weld metal and slag crust. Ibid., 2, 1–4.
6. Podgaetsky, V.V., Kuzmenko, V.G. (1988) Welding slags. Kiev: Naukova Dumka.
7. Volobuev, O.S., Potapov, N.N., Volobuev, Yu.S. et al.
(1989) To the problem of influence of linear expansion coefficient on slag crust detachability. Svarochn. Proizvodstvo, 8, 37–39.
8. Bobrikov, Yu.V., Potapov, N.N., Starchenko, E.G. (1983) Peculiarities of metal oxidation by zirconium dioxide in submerged-arc surfacing. Ibid., 9, 6–7.
9. Potapov, N.N. (1985) Oxidation of metals in fusion welding. Moscow: Mashinostroenie.
10. Ryabtsev, I.I. (2005) Improvement of slag crust detachability at higher temperatures in flux-cored wire submerged-arc surfacing. In: Proc. of Sci.-Techn. Conf. of Junior Scientists on Welding and Related Technologies (Kiev, 25--27 May, 2005). Kiev: PWI, 59–60.
11. Bondarenko, T.P., Rimsky, S.T., Zalevsky, A.V. et al. (1991) Procedure of measurement of reactivity and pressure of oxygen in fluxes. In: Welding consumables for mechanized arc welding of steels. Kiev: PWI.
12. Kolisnyk, V.N., Shono, S.A., Saginov, I.A. Rotational viscometer. USSR author’s cert. 667867. Int. Cl. G 01 11/14. Publ. 15.06.79.
13. Rietveld, H.M. (1969) A profile refinement method for nuclear and magnetic structures. J. Appl. Cryst., 2, 65–71.
14. Kovba, L.M. (1991) Radiography in inorganic chemistry: Manual. Moscow: MGU.
15. Berezhnoj, A.S. (1970) Multicomponent systems of oxides. Kiev: Naukova Dumka.

Suggested Citation

V.E. Sokolsky, A.S. Roik, V.P. Kazimirov, I.I. Ryabtsev, D.D. Mishchenko, I.A. Ryabtsev, A.S. Kotelchuk, V.S. Tokarev (2008) Effect of zirconia on properties of slag in flux-cored wire submerged-arc surfacing using flux AN-348A. The Paton Welding J., 07, 19-23.