TPWJ, 2010, #6, 22-25 pages
 
ELIMINATION OF UNDERCUTS IN EBW WITH COMPLETE AND INCOMPLETE PENETRATION


Journal                    The Paton Welding Journal
Publisher                 International Association «Welding»
ISSN                       0957-798X (print)
Issue                       № 6, 2010 (June)
Pages                      22-25
 
 
Authors
L.A. KRAVCHUK

E.O. Paton Electric Welding Institute, NASU, Kiev, Ukraine
 
 
Abstract
Some peculiarities of formation of crater and weld pool in electron beam welding of 17 mm thick titanium alloy VT20 with complete and incomplete penetration in different positions are considered. Welding schematics and parameters providing defect-free formation of the face and reverse weld beads are given.
 
 
Keywords: electron beam welding. titanium alloys, electron beam, welding schematic, weld pool, defects, crater, face and reverse weld beads
 
 
Received:                ??.??.??
Published:               28.06.10
 
 
References
1. Stocker, G. (1974) Erfahrungen beim Elektronenstrahlschweissen dickwandiger Bauteile aus der Titanlegierung Ti-6Al-4V geglueht. Schweissen und Schneiden, 26(9), 91-93.
2. Paton, B.E., Nazarenko, O.K., Nesterenkov, V.M. et al. (2004) Computer control of electron beam welding with multi-coordinate displacements of the gun and workpiece. The Paton Welding J., 5, 2-5.
3. Wiesner, P., Ehrhard, H. (1983) Elektronenstrahlschweissen mit Strahlpendeln. ZIS Mitteilungen, 25(1), 17-28.
4. Friedel, K.P., Arata, Y. (1980) Preliminary evaluation of root defects elimination methods in partial penetration EB welding. In: Proc. of Int. Conf. on Welding Research (Oct. 27-29, 1980, Osaka), Section F.
5. Paton, B.E., Nazarenko, O.K., Lokshin, V.E. et al. (1972) Peculiarities of electron beam welding in different spatial positions. Avtomatich. Svarka, 6, 1-4.
6. Nudelman, Ya.B., Zadery, B.A. (1988) Weld formation in electron beam welding of up to 25 mm thick titanium alloys. Ibid., 5, 29-30.