The Paton Welding Journal, 2023, #6, 18-23 pages
Narrow-gap TIG welding of thick steel 20
S.V. Akhonin, V.Yu. Bilous, R.V. Selin, V.V. Pashynskyi, S.L. Shvab
E.O. Paton Electric Welding Institute of the NASU.
11 Kazymyr Malevych Str., 03150, Kyiv, Ukraine. E-mail: belousvy@gmail.com
Abstract
Arc welding of joints of carbon steels 20...100 mm thick can be performed both by consumable and nonconsumable electrode,
using shielding gases or flux. In order to increase the efficiency of welding operations, multilayer narrow-gap welding with
filler wire feeding can be used for metals of medium and large thicknesses. This study deals with application of narrow-gap
tungsten electrode welding with and without application of a controlling magnetic field for welding samples from steel 20 of
40 mm thickness. Results of investigations of the macro- and microstructure and microhardness of the welded joints are given.
It was found that application of an external magnetic field for narrow-gap welding of steel 20 joints ensures a higher quality of
the welded joints. 14 Ref., 8 Fig.
Keywords: narrow-gap argon-arc welding, tungsten electrode, steel 20, controlling magnetic field, structure, microstructure,
microhardness
Received: 16.05.2023
Accepted: 17.07.2023
References
1. Akhonin, S.V., Belous, V.Yu., Romanyuk, V.S. et al. (2010) Narrow-gap welding of up to 110 mm thick high-strength titanium alloys. The Paton Welding J., 5, 34-37.
2. Malin, V. (1987) Monograph on Narrow-Gap Welding Technology. WRC, Bulletin 323.
3. Hori, K., Haneda, M. (1999) Narrow gap arc welding. J. of J.W.S, 3, 41-62.
https://doi.org/10.2207/qjjws1943.68.1794. Jun, J.H., Kim, S.R., Cho, S.M. (2016) A Study on Productivity Improvement in Narrow Gap TIG Welding. Journal of Welding and Joining, 34 (1), 68-74.
https://doi.org/10.5781/JWJ.2016.34.1.685. Dak, G., Khanna, N., Pandey, C. (2023) Study on narrow gap welding of martensitic grade P92 and austenitic grade AISI 304L SS steel for ultra-supercritical power plant application. Archiv. Civ. Mech. Eng. 23, 14-24.
https://doi.org/10.1007/s43452-022-00540-36. Luo, Y., Zhang, Z.L., Zhou, C.F. et al. (2017) Effect of oscillation parameters of narrow groove MAG welding on weld formation. J. Hebei Univ. Sci. Technol, 38, 6. https:// doi.org/10.7535/hbkd.2017yx01002
7. Nguyen, D.H. (2014) Research on Droplet Transfer and Welding Process of Oscillation arc Narrow Gap GMAW. Master's Thesis, Harbin Institute of Technology, Harbin, China.
8. Fang, D.S. (2017) Study on the Characteristics of Three-Wire Indirect arc and Its Thick-Wall Narrow Gap Welding Process under Gas Protection. Ph.D. Thesis, Dalian University of Technology, Dalian China.
9. Shoichi, M., Yukio, M., Koki, T. et al. (2013) Study on the application for electromagnetic controlled molten pool welding process in overhead and flat position welding. Sci. Technol. Weld. Join. 18, 38-44.
https://doi.org/10.1179/1362171812Y.000000007010. Belous, V.Yu., Akhonin, S.V. (2007) Influence of controlling magnetic field parameters on weld formation in narrow-gap argon-arc welding of titanium alloys. The Paton Welding J., 4, 2-5.
11. Xinyu, B., Yonglin, M., Shuqing, X. et al. (2022) Effects of Pulsed Magnetic Field Melt Treatmenton Grain Refinement of Al-Si-Mg-Cu-Ni Alloy Direct-Chill Casting Billet. Metals, 12(7), 1080.
https://doi.org/10.3390/met1207108012. Yujun, H., Hongjin, Z., Xuede, Y. et al. (2022) Research Progress of Magnetic Field Regulated Mechanical Property of Solid Metal Materials, Metals, 12, 1988.
https://doi.org/10.3390/met1211198813. Pashynskaya, E.G., Pashynskiy, V.V. (1998) Effect of weakpulsed magnetic field on structure and properties of Cu-Sn base alloy. Physic of Metals and Metallography, 6, 670-674.
14. Belous, V.Yu., Akhonin, S.V. (2011) Formation of narrowgap welded joints on titanium using the controlling magnetic field. The Paton Welding J., 4, 19-22.
Suggested Citation
S.V. Akhonin, V.Yu. Bilous, R.V. Selin, V.V. Pashynskyi, S.L. Shvab (2023) Narrow-gap TIG welding of thick steel 20.
The Paton Welding J., 06, 18-23.