The Paton Welding Journal, 2022, #7, 23-27 pages

Effectiveness of combined gas-slag protection at mig deposition of copper alloys on steel

T.B. Maidanchuk, V.M. Ilyushenko, A.M. Bondarenko, D.M. Stepchenko


E.O. Paton Electric Welding Institute of the NASU. 11 Kazymyr Malevych Str., 03150, Kyiv, Ukraine. E-mail: pwi_37@ukr.net

Abstract
A complex of investigations was performed to study the technological capabilities for application of combined gas-slag protection in MIG-process of copper alloy deposition on steel. It is shown that at semi-submerged arc surfacing (by semi-open arc) it is possible to control the technological characteristics of the welding arc, namely: increase its spatial stability, improve the pattern of electrode metal transfer (essentially reducing its spattering fraction), as well as ensure high-quality protection of the deposits from oxidation. Application of such a combined protection is particularly rational at highly efficient process of two-electrode MIG surfacing. 7 Ref., 1 Tabl., 7 Fig.
Keywords: copper alloys, combined gas-slag protection, spatial stability of the arc, two-electrode surfacing, deposited metal quality

Received: 17.05.2022
Accepted: 15.09.2022

References

1. Gurevich, S.M. (1990) Handbook on welding of nonferrous metals. Kyiv, Naukova Dumka [in Russian].
2. Ilyushenko, V.M., Lukyanchenko, E.P. (2013) Welding and surfacing of copper and copper alloys. Kyiv, IAW [in Russian].
3. Kittichai Sojiphan, Trinet Yingsamphancharoen, Narawit Paosen et al. (2019) Effects of MIG-brazing current on wettability and mechanical property of galvanized steel lap joints. In: Proc. of 12th Int. Conf. on Thailand Metallurgy, 93–99. DOI: 10.13140/RG.2.2.30625.56162
4. https://www.fronius.com/en-us/usa/welding-technology/ world-of-welding/fronius-welding-processes/cmt
5. Pokhodnya, I.K. (1990) Metallurgy of arc welding. Processes in arc and melting of electrodes. Kyiv, Naukova Dumka [in Russian].
6. Shlepakov, V.N., Kotelchuk, A.S. (2019) Improvement of technological and sanitary-hygienic characteristics of gas-shielded arc welding process. The Paton Welding J., 6, 29-33. https://doi.org/10.15407/as2019.06.05
7. Bonnel, J.-M., Maurer, M., Rosert, R. (2019) Submerged arc surfacing of high-alloy steels by flux-cored wires. The Paton Welding J., 6, 3-12 https://doi.org/10.15407/as2019.06.01

Suggested Citation

T.B. Maidanchuk, V.M. Ilyushenko, A.M. Bondarenko, D.M. Stepchenko (2022) Effectiveness of combined gas-slag protection at mig deposition of copper alloys on steel. The Paton Welding J., 07, 23-27.